產品參數
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 |
霧度2 | 40 mil | ASTM D-1003 | 76.1 | % |
硬度2 | Shore A 15 sec | ASTM D-2240 | >90 | |
密度 | ExxonMobil Method0.902g/cm3 | |||
熔體流動速率 | ExxonMobil Method2.5g/10 min | |||
硬度2 | Shore D 15 sec | ASTM D-2240 | 36.8 | |
熔融指數 | ExxonMobil Method1.1g/10 min | |||
彎曲模量 | 1% secant | ASTM D-790 | 9842(67.9) | psi(MPa) |
沖擊強度 | 23℃ | ASTM D-256 | No Break | ft-lb/in(J/m) |
沖擊強度 | -40℃ | ASTM D-256 | No Break | ft-lb/in(J/m) |
拉伸強度3 | @Break | ASTM D-638 | No Break | psi(MPa) |
拉伸率 | @Break | ASTM D-638 | No Break | % |
最高熔體溫度 | ExxonMobil Method206.4(96.9)?H(℃) | |||
維卡軟化點2 | 1000g | ASTM D-1525 | 182.7(83.7) | H(℃) |
維卡軟化點2 | 200g | ASTM D-1525 | 205.2(96.2) | H(℃) |
拉應力5 | @100% Elongation | ASTM D-412 | 1780(12.3) | psi(MPa) |
拉伸率 | @Break | ASTM D-412 | 1144 | % |
抗扯強度 | ASTM D-624508.5(89.1)lb-in(kN/m) | |||
拉伸強度 | @Peak | ASTM D-412 | 4454(30.7) | psi(MPa) |
門尼粘度ML(1+4) | 125℃ | ASTM D-1646 | 3.9 | Torgue Units |
抗環境應力開裂性 | ASTM D-1693>1000hr | |||
拉應力5 | @300% Elongation | ASTM D-412 | 2115(14.6) | psi(MPa) |